| Title | ZnO as transparent conducting oxide by Atomic Layer Deposition |
| Publication Type | Conference Paper |
| Year of Publication | 2013 |
| Authors | Sinha, S., and S. K. Sarkar |
| Conference Name | Conference Record of the IEEE Photovoltaic Specialists Conference |
| URL | https://www.scopus.com/inward/record.uri?eid=2-s2.0-84896462360&doi=10.1109%2fPVSC.2013.6744351&partnerID=40&md5=c7c8baa799c1ae871e33708101dbe999 |
| DOI | 10.1109/PVSC.2013.6744351 |