| Title | Atomic layer deposition of amorphous antimony sulfide (a-Sb2S3) as semiconductor sensitizer in extremely thin absorber solar cell |
| Publication Type | Journal Article |
| Year of Publication | 2020 |
| Authors | Mahuli, N., D. Halder, A. Paul, and S. K. Sarkar |
| Journal | Journal of Vacuum Science and Technology A: Vacuum, Surfaces and Films |
| Volume | 38 |
| URL | https://www.scopus.com/inward/record.uri?eid=2-s2.0-85082579452&doi=10.1116%2f6.0000031&partnerID=40&md5=d8ddaacc1f34b05c575c9a0f8ec857aa |
| DOI | 10.1116/6.0000031 |